TPU Nanocomposite

Patent Title: POLYURETHANE COMPOSITE

 Number/Link: WO2018/185650 (Spanish)

Applicant/Assignee: UNIVERSIDAD DE ANTIOQUIA

Publication date: 11 October 2018

Gist”: Protein-stabilized nano- calciumcarbonate particles are incorporated into a thermoplastic polyurethane composition

Why it is interesting: Calciumcarbonate nanoparticles are prepared by mixing a solution of sodium carbonate, sodium caseinate and calciumchloride in a high pressure homogenizer. Particles are formed of CaCO3 embedded in a protein matrix that stabilizes that particles against aggregation. Particle size is (pref) 150-300nm with primary CaCO3 particles of 5-10nm. The particles are used in an amount of (pref) 0.6-1% (w/w) on a TPU composition. The TPUs are said to show increased mechanical properties and improved cell growth and are said to be useful for biomedical applications.

nanoparticle

Stabilized nanoparticles (Wikipedia)

Thermoreversible Polyurea

Patent Title: DYNAMIC UREA BONDS FOR POLYMERS

 Number/Link: W02016/069582

Applicant/Assignee: University of Illinois

Publication date: 6-05-2016

Gist”: Urea bonds prepared from sterically hindered amines and isocyanates

Why it is interesting: The N-C bond in urea is very stable due to conjugation of the lone electron pair of the nitrogen atom with the cabonyl group.  According to this invention, the nitrogen atom can be subsituted with a strongly hindering group such that the coplanarity, and therefore most of the conjugation, of the C-N and C=O bonds is lost. These hindered urea bonds are much less stable and can reversibly depolymerize at relatively low temperatures. Thermoreversible bonds can be useful in a number of smart materials such as self-healing-, “4D printing”- , and reprogrammable shape memory materials. In an example a shape memory material with a Tg of 53°C and a Young’s Modulus of about 2 GPa was prepared by reacting 2-(t-buylamino)ethanol (TBAE) and trimerized hexamethylene diisocyanate (THDI). The ‘permanent shape’ of the material could be re-programmed by forcing the material in a new shape for 72 hours at 60°C.

Polurethane-urea with thermoreverisble urea bonds

Poly(urethane-urea) with thermoreverisble urea bonds